WebFeb 24, 2005 · I use a 50/50 mix of ferric cloride to water and etch for 10 min, neutralize in tri sodium phosphate. I shoot for the temp of the acid/water solution to be about 70f. The warmer the acid the faster the etch. If the acid is cold it will take forever to etch the blade, if the acid is hot it will eat the steel up quickly. WebSep 3, 2024 · To etch, first sand — but do not buff — your Damascus blade. Wash your sanded blade with alcohol and dry with a clean cloth. Prepare your solution by mixing ferric chloride with distilled water, then warm it to room temperature if needed.

Damascus not etching. KnifeDogs.com Forums

WebBS110 Ferric Chloride for Acid Etching Damascus Used to acid etch Damascus after heat treating. 16oz makes one half gallon of usable solution. Dilute with distilled water. Keep bottle tightly sealed and stored … WebUsing Ferric Chloride to Etch Damascus Steel - Artist Blacksmith cs7001iaw 9 https://womanandwolfpre-loved.com

Etching Damascus? Ferric Chloride Container How To

WebMay 14, 2024 · Generally speaking, you want to be at about a 400 grit finish or better to get an even etch across the pattern. If you are having trouble getting Ferric, try using … WebApr 27, 2024 · Ferric chloride will etch stainless damascus, just takes a little longer. Mark Barone Well-Known Member. Apr 25, 2024 #16 Mystery solved. The acid was contaminated somehow. I finally received a new bottle and it worked well on my piece. I wish I knew what contaminated it. I probably did about 4 knives in it. WebFerric chloride is a traditional home-use circuit board etchant. It's easy enough to come by, and the Ferric by itself is no big environmental problem. However, once you've etched a … cs7001iw

Etching 101: How To Etch Your Damascus Pattern Welded Blade

Category:Damascus Etch: What have I done wrong?

Tags:Ferric chloride for etching damascus

Ferric chloride for etching damascus

Etching Damascus? Ferric Chloride Container How To - YouTube

WebJun 26, 2024 · The particulars: 11 layer 80CrV2 and 15N20. Slow twist. Hand hammered. Welded perfectly, no flux. Rough ground to 220 ish, coated in Turco, normalize, thermal cycled, quench in 10 sec commercial … WebMay 11, 2024 · Damascus etching is completed with either ferric chloride or muriatic acid. Before you begin, check the expiration date on your acid of choice to be sure that it’s not too old. Using expired acid causes problems with your etch, and you don’t want to … Properly annealing, heat treating, and tempering a piece of Damascus is an … Vegas Forge produces the finest Damascus steel for sale with a focus on … Preheat: Heat to 1400°F (760°C) Equalize. Austenitize: 2050°F, hold time at … Damascus End Cuts (Box O Scraps) Footer. Company. About Us; Blog; …

Ferric chloride for etching damascus

Did you know?

WebA follow up to the video "Damascus 101", taking you step by step through the process of etching a damascus blade after the forging and heat treating process.... WebThis is the process I use to make my own ferric chloride for etching San Mai and Damascus knife blades. The ratio is fairly simple, 2 parts hydrogen peroxide...

WebJan 10, 2014 · I bought some Damascus to try out on a few blade designs.The etching directions said to use Ferric Chloride to bring out the pattern. I tried Radio Shack for … WebDec 1, 2007 · I want to etch a Damascus hawk head, and I don't know where to get ferric chloride. I know my local radio shacks don't have it. And I would rather not pay the $20 HazMat fee, anyone know a good online source for (preferably) powdered FeCl? Thanks! edit: Also, I don't really need all that much...

WebSep 3, 2024 · Finally, submerse your blade into the ferric chloride-water solution for 10-15 minutes, gently brushing the piece to remove the dissolving material. When you're done … WebAug 24, 2024 · First I ferric chloride etch for a couple minutes, rinse, then go right into the coffee for 6 or 8 hours. I am getting a bad yellow Hugh on the migration line and I want it to be that cool bright silver. I have went back into the ferric after the coffee and that seems to help brighten things up.

WebThe meaning of FERRIC CHLORIDE is a deliquescent dark salt FeCl3 that readily hydrates to the yellow-orange form and that is used especially for etching, in sewage treatment, …

WebFerric chloride is one of the most widely used etchants in the field of chemical etching. It is commonly used to etch steel and stainless steel parts, but it is also capable of etching … dynarex ink capsWebMay 9, 2024 · For so long ive used a variety of containers to store my ferric chloride so i finally decided to build a proper storage container.Please SUPPORT me on PATREO... cs7001i aw 17 or-tWebMar 9, 2024 · Choose the acid you want to etch the steel with. Possible acids include muriatic (hydrochloric) acid (HCL), nitric acid (HNO3), or sulfuric acid (H2SO4). Certain … dynarex hypodermic needleshttp://artmondo.net/printworks/articles/ferric.htm cs7001iaw 9 or-sWebJul 25, 2024 · Etching Damascus with Ferric Chloride - YouTube Etching the Winter’s Edge Bowie with Ferric Chloride. Etching the Winter’s Edge Bowie with Ferric Chloride.... dynarex instant coldWebStep 1: What You'll Need. Making ferric chloride is relatively simple. Here's what you need: Muriatic Acid (Hydrochloric Acid) 0000 Steel Wool. Hydrogen Peroxide (6% or higher … cs7000 brother sewing machineWebOct 31, 2014 · When I am etching any kind of stainless steel Damascus its time to use mix a batch of Ferric Chloride out in the shop because stales will laugh at vinegar as an … dynarex instant cold pack weight